Euroengel obtains the qualification of welding procedures from IIS

Euroengel srl gets the qualification of welding procedures and operators at the Italian Welding Institute (IIS), through the partner AQM. The certification, issued in compliance with the main international standards, concerns one of the key processes in the production of the Coldtainer range: the hermetic refrigeration circuit. This certification encourages us to continue on this path, working to achieve the highest quality standards.